New product
1.1 This test method establishes a procedure to measure the susceptibility of steel to a time-delayed failure such as that caused by hydrogen. It does so by measuring the threshold for the onset of subcritical crack growth using standard fracture mechanics specimens, irregular-shaped specimens such as notched round bars, or actual product such as fasteners (2) (threaded or unthreaded) springs or components as identified in SAE J78, J81, and J1237.
| Author | ASTM |
|---|---|
| Editor | ASTM |
| Document type | Standard |
| Format | File |
| Confirmation date | 2018-11-01 |
| ICS | 77.040.10 : Mechanical testing of metals
|
| Number of pages | 12 |
| Replace | ASTM F1624-12 |
| Set | ASTMVOL1503 |
| Year | 2012 |
| Document history | ASTM F1624-12 |
| Country | USA |
| Keyword | ASTM 1624;ASTM F1624;ASTM F1624;10.1520/F1624-12R18 |