1.1 This test method describes the requirements for sample preparation and tensile testing of single-lap shear splices formed with fiber-reinforced polymer (FRP) composite materials commonly used for strengthening of structures made of materials such as metals, timber, masonry, and reinforced concrete. The objective of this method is to determine the apparent shear strength of an overlap splice joint through the application of a far-field tensile force. The method applies to wet lay-up FRP material systems fabricated on site or in a laboratory setting. The FRP composite may be of either unidirectional (0°) or cross-ply (0/90 type) reinforcement. For cross-ply laminates, the construction may be achieved using multiple-layers of unidirectional fibers at either 0 or 90°, or one or more layers of stitched or woven 0/90 fabrics. The composite material forms are limited to continuous fiber or discontinuous fiber-reinforced composites in which the laminate is balanced and symmetric with respect to the test direction. The method is often used to determine the length of the overlap splice needed to ensure that a tension failure occurs in the material away from the splice rather than the splice connection itself.

Author ASTM
Editor ASTM
Document type Standard
Format File
Confirmation date 2017-08-01
ICS 83.180 : Adhesives
Number of pages 7
Replace ASTM D7616/D7616M-11
Set ASTMVOL1503
Year 2011
Document history ASTM D7616/D7616M-11
Country USA
Keyword ASTM 7616;ASTM D7616;ASTM D7616;10.1520/D7616_D7616M-11R17