FORD WRS-M4D1058-A1 2015 Edition, October 1, 2015
POLYPROPYLENE (PP) MOLDING COMPOUND, HOMOPOLYMER, HEAT STABILIZED, 35%
GLASS FIBER/MINERAL REINFORCED, 100% PCR/PIR RESIN CONTENT, 65% RECYCLED
MATERIAL BY WEIGHT, NON-VISIBLE APPLICATIONS ***TO BE USED WITH FORD
WSS-M99P1111-A***
Description / Abstract:
The material defined by this specification is based on a 25%
glass fiber and 10% mineral reinforced thermoplastic injection
molding compound, with 100% recycled resin